Air Plasma Spray Titanium Coatings
With different thickness and roughness levels, APS Ti coatings are suitable for several kinds of medical devices
With different thickness and roughness levels, APS Ti coatings are suitable for several kinds of medical devices.
Low roughness Ti-coatings are tipically used to coat dental implants and spinal components, while high roughness Ti-Coatings are used on joint components.
Y 371

| Suggested thickness | 20 -100 μm |
|---|---|
| Adhesion strength | ≥ 45 MPa |
| Porosity | 4 -7 % |
| Roughness (Rt) | 40 - 80 μm |
Y 367

| Suggested thickness | 150 - 350 μm |
|---|---|
| Adhesion strength | ≥ 30 MPa |
| Porosity | 20 - 40 % |
| Roughness (Rt) | 90 -170 μm |
Excellent biocompatibility has been established for both the coatings through in-vitro characterization

Osteoblast cells growing proliferation trend

Ti Growth®
The first titanium sponge applicable to prostheses made with thermal spray technologyVacuum Plasma Spray Titanium Coatings
High levels of purity, increased adhesion strenght, roughness and porosity
Hybrid Plasma Spray Titanium Coatings
Your choice when efficiency is the goal
Coating on Peek
The basis for the development of a PS coating family (Spondycoat®) for PEEK-based components